Lime fononoo a ɛkyinkyini no mu titiriw yɛ fononoo a ɛyɛ kurukuruwa tenten bi a ɛkɔ fam kakra. Wɔde dade a ɛyɛ papa-ayɛ, na wɔde nneɛma a ɛyɛ hyew a ɛko tia ɔhyew a ɛkorɔn-ahyɛ fononoo no mu wɔ ne mu fasu no so, a wɔde ntwahonan a wɔte so no nhyiam ahorow gyina akyi, na wɔde ntwahonan nhyehyɛe a wɔde fa nneɛma mu (a ahoɔhare a wɔtaa di akɔneaba yɛ 1–4 r/min) na ɛma ɛkyinkyini brɛoo. Mpɛn pii no, wɔde nnwinnade a ɛboa a nea ɛka ho ne preheater, cooler, burner, ne mfutuma a wɔboaboa ano hyehyɛ nhyehyɛe a edi mũ no mu, na ɛyɛ nhyehyɛe a wɔaka abom a ɛkɔ so yɛ hyew.
N’adwuma nnyinasosɛm di ntease titiriw a ɛne ɔhyew a ɛsesa ne gradient calcination akyi. Wobetumi akyekyɛ adeyɛ no mu ayɛ no afã atitiriw abiɛsa:
1.Aduan ne Preheating Stage
Limestone a wɔde yɛ nneɛma no fa afiri a wɔde ma aduan no so hyɛn preheater no mu na ɛkɔ brɛoo kɔ fam awiei (kiln hood) wɔ tumi a ɛtwe ade ba fam ase bere a fononoo no di akɔneaba no. Saa bere yi nyinaa, mframa a ɛyɛ hyew-a ɛkorɔn a ɛnam pɛtro (fango a wɔabɔ no apete, abɔde mu mframa, ne nea ɛkeka ho) a wɔde fi fononoo no ano hyew mu no mu ba no sen fa fononoo no so wɔ axially fi fononoo no anim kɔ fononoo no dua no so. Wɔ saa nsuo a ɛsen yi mu no, ɔhyeɛ nsakraeɛ a ɛdi kan ba wɔ mframa a ɛfiri afiri mu ne counter{4}}adeɛ a ɛtu no ntam, na ɛma nneɛma no hyeɛ kɔ soro nkakrankakra ma nsuo a ɛyɛ nwini wie na ɛsiesie ne ho ma carbonate a ɛdi kan yɛ hyew na ɛporɔw.
2.Calcination ne Porɔw Stage
Bere a ade no hyɛn beae a ɛhɔ yɛ hyew kɛse-wɔ fononoo no mfinimfini (ɔhyew a ɛkɔ soro kodu 1200–1400 °C) no, ɛne mframa a ɛwɔ ɔhyew a ɛkorɔn-mu no di nkitaho koraa bere a ɛkɔ so ne fononoo no kyinhyia no. Limestone (CaCO3) porɔw kɛse ma ɛyɛ quicklime (CaO) ne carbon dioxide (CO2). Tumbling a ɛkɔ so no hwɛ hu sɛ ɔhyew a ɛyɛ pɛ, siw ano yiye wɔ -calcination anaasɛ over{1}}calcination locally-eyi ne ade titiriw nti a nneɛma no yɛ papa wɔ rotary fononoo mu.
3.Cooling ne Discharging Stage
Quicklime a wɔahyew no kɔ so kɔ fononoo no ano na ɛhyɛn cooler a ɛne no hyia no mu, baabi a ɛne mframa a ɛyɛ nwini a wɔabɔ-sesa ɔhyew. Wɔma quicklime no dwo kodu baabi a ɛhɔ yɛ hyew na wɔtow gu, bere a mframa a ɛyɛ nwini no, bere a agye ɔhyew akyi no, ɛbɛyɛ mframa a ɛyɛ hyew; wobetumi asan de ne fã bi adi dwuma sɛ ɔhyew-a ɛboa mframa a ɛsan kɔ fononoo no hood no mu ma ɔhyew san ba. Awiei koraa no, wɔtow mframa a ɛyɛ hyew a ɛkɔ soro-fi fononoo no dua mu, na wɔde mfutuma a woyi fi mu, de sulfurization, ne denitrification di ho dwuma ma ɛne nneɛma a atwa yɛn ho ahyia gyinapɛn ahorow hyia ansa na wɔayi afi mu.

 